EC 130 LV epoxy resin + W 341 hardener 1+0,3 kg

EC 130 LV epoxy resin + W 341 hardener 1+0,3 kg
  • EC 130 LV epoxy resin + W 341 hardener 1+0,3 kg
Mixing ratio (by weight):
100:30
Weights (kg) select:
Demoulding time (at 25 ° C):

Epoxy laminating resin system for composites with high thermal resistance.





  • Manual impregnation at atmospheric pressure or under vacuum bag for wood, glass, carbon or kevlar fiber tissue. Room temperature curing. The hardeners can be blended in all proportions to adjust the reactivity of the system to the specific needs. Compared to traditional systems, this one also presents an high capability to post-cure also with a moderate heat transfer.

    W 340 (medium-slow): Under vacuum impregnation.

    W 341 (fast): Impregnation by contact and medium size components.

  • Processing time
    10-15 min
    Demoulding time (at 25 ° C)
    15-20 hours