EC 130 LV epoxy resin + W 342 hardener 1+0,3 kg
Gross: 11 661 Ft/pcs
EC 130 LV epoxy resin + W 342 hardener 1+0,3 kg
Gross: 11 661 Ft/pcs
Unit price: Gross: 8 970 Ft/kg
Mixing ratio (by weight):
100:30
Demoulding time (at 25 ° C)
Demoulding time (at 25 ° C):
High performance composite parts of small and medium size. Structural parts for boats, model aircrafts, racing vehicles, sport components.
Details
Under vacuum impregnation, manual at atmospheric pressure and under vacuum bag for wood, glass, carbon or kevlar fiber tissue. Room temperature or moderate temperature curing. Un-filled epoxy system.
The system EC 130LV/W 342 allows the obtainment of a good surface finish. Very good resistance towards UV. Good thermal resistance. The post-curing at a moderate temperature is suggested to obtain the best performance for the system.
Data
Processing time:
22-27 min
Demoulding time (at 25 ° C):
12-17 hours
Weight:
1.6 kg/pcs
Reviews